With tensile strengths comparable to that of 304, MP35N is double melted in order to give this alloy its exceptional combination of strength and corrosion resistance.
ASTM F562 | |
Carbon | 0.025 |
Manganese | 0.15 |
Silicon | 0.15 |
Phosphorus | 0.015 |
Sulfur | 0.01 |
Chromium | 19.00-21.00 |
Nickel | 33.00-37.00 |
Molybdenum | 9.00-10.50 |
Cobalt | Balance |
Titanium | 1 |
Iron | 1 |
Boron | 0.015 |